• Become a Subscribing Member today!

    The Biplane Forum is a large global active community of biplane builders, owners and pilots. From Pitts to Skybolts, to older barnstormers, all types are welcome.

    The Biplane Forum is a private community. Subscriptions are only $49.99/year or $6.99/month to gain access to this great community and unmatched source of information not found anywhere else on the web.

    Why become a Subscribing Member?

    • In addition to our active community, our content boasts exhaustive technical information which is often sought after for projects and maintenance. This information has accumulated over the 12+ years the forum has been in existence.
    • We are also a great resource for non biplane users, since many GA aircraft are built the same way (fabric and tube construction).
    • Annual membership also comes with two BiplaneForum.com decals.

    Become a Subscribing Member and access the Biplane Forum in full!

    Subscribe Now

Composite core material

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Joined
Jun 16, 2013
Messages
954
Reaction score
458
Location
Fargo, ND
I'm trying to form PVC core material for my Skybolt side panels. Specs say 200* air for 10 mins with the center temp being 175*.
I have tried 500W halogen lights, hot water, 2 heat guns. So far all I've accomplished is overheating/charring one end of a block. Currently using a 30x32x8 inch box made from 2" Styrofoam insulation.
Anyone have suggestions on heating?

edit: I forgot, this is 1" thick PVC core. Trade name Divinyacore.
 