• The Biplane Forum is a large global active community of biplane builders, owners and pilots. From Pitts to Skybolts, to older barnstormers, all types are welcome. In addition to our active community, our content boasts exhaustive technical information which is often sought after for projects and maintenance. This information has accumulated over the 12+ years the forum has been in existence.

    The Biplane Forum is a private community. Subscriptions are only $49.99/year or $6.99/month to gain access to this great community and unmatched source of information not found anywhere else on the web. We are also a great resource for non biplane users, since many GA aircraft are built the same way (fabric and tube construction). Annual membership also comes with two BiplaneForum.com decals.



Weld crack, whats up?

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

DragonflyDH90

Well-Known Member
*
Joined
Oct 5, 2007
Messages
711
Reaction score
112
ThoughtI would run this past those on the forum and get some opinions.
Hydrogen cracking? hot weld stress crack?
It is a little hard to see from the pic but the area could potentially be slightly undercut.


This has not happened in service as it is on a new doubler plate on the bottomrear wing attach fitting.


Idont know if it occured as the weld cooled or over a time period after.


What do you think is the best repair method here?


20120304_032415_IMAG0036.jpg